Wood Grain Effect Thermoset Powder Coating paint For Aluminum Profiles
1. Operation Manual For wooden effect heat transfer with glue
1. After the normal spraying base powder, then baking,but the baking time should be 3-5 minutes longer than ordinary powder baking ,to ensure that the film fully cured, this is conducive to the transfer paper peel off . The normal requirements for indoor use powder 180℃-190℃ ,20-25 minutes, 12-17 minutes 200-205 degrees for outdoor use powder. According to the customer’s oven conditions adjustment. Particular attention that 180-190 degrees is the surface temperature of the workpiece, not the temperature of the air in the oven. It means when your workpiece surface temperature reach 180--190 degrees, then baking 20-25 minutes.
2. After the cooling of the powder, roll coating a layer of uniform diameter dilution to the appropriate proportion glue ,(Transfer glue: water =1:7 or so, stirring with a slight greater than the water resistance is appropriate),Thickness to wet transfer printing paper is appropriate, then cut right size transfer paper alignment paste is good and very thin PVC membrane paper rubbing pressure, squeeze out excess glue,With an art knife gently along the bottom of the pattern on the transfer printing paper, so that the paper is completely affixed to the prison.baking with 150-160 degrees,5-8 minutes transfer (to avoid strong winds) and stay cool and spilled transfer paper, available after the blisters erase residual scraps of paper.
3. After cleaning, dry water, If there is residual glue watermark ,baking again with 120 degrees 5 minutes ,to remove traces of glue.
4. if necessary, then spray transparent light oil (cover light oil).
2. THE ADVANTAGES OF Hsinda :
|
|
|
|
|
|
|
3. the Advance of Hsinda Products
better resin from DSM | better pigment provide a good voverage and weather resist |
higher coverage | lower necessary thickness |
higher resin percentage | stable quality for each order |
the Advance of Hsinda Services
products customize |
7*24 hours online |
comprehensive cost analysis |
powder coating quality control system build |
Application
Electrical Household Appliances | Aerospace Area |
Automotive Electronics | Fitness Equipment |
Track Traffic | Medical Devices |
Petroleum Pipes, Valve | Tools & Hardware |
LED Lights, Outdoor Lamps | Radiator & Heat Sink |
Glass Decoration | External Facilities |
Powder Coating Spray
FAQ
1, what's the moq for the first time ?
for the first time , any quantity will be acceptable , but to save your ship cost . few kgs will be good. formal order moq will be 300kg per color .
2, could you do OEM for us ?
yes , we can do OEM for a distributor if you want , but may require a order more than 10 tons.
Brand Name: | Hsinda |
Model Number: | wood grain |
MOQ: | 300kg |
Price: | Negotiable |
Packaging Details: | Inner packing : paper carton |
Payment Terms: | L/C, T/T, Western Union |
Wood Grain Effect Thermoset Powder Coating paint For Aluminum Profiles
1. Operation Manual For wooden effect heat transfer with glue
1. After the normal spraying base powder, then baking,but the baking time should be 3-5 minutes longer than ordinary powder baking ,to ensure that the film fully cured, this is conducive to the transfer paper peel off . The normal requirements for indoor use powder 180℃-190℃ ,20-25 minutes, 12-17 minutes 200-205 degrees for outdoor use powder. According to the customer’s oven conditions adjustment. Particular attention that 180-190 degrees is the surface temperature of the workpiece, not the temperature of the air in the oven. It means when your workpiece surface temperature reach 180--190 degrees, then baking 20-25 minutes.
2. After the cooling of the powder, roll coating a layer of uniform diameter dilution to the appropriate proportion glue ,(Transfer glue: water =1:7 or so, stirring with a slight greater than the water resistance is appropriate),Thickness to wet transfer printing paper is appropriate, then cut right size transfer paper alignment paste is good and very thin PVC membrane paper rubbing pressure, squeeze out excess glue,With an art knife gently along the bottom of the pattern on the transfer printing paper, so that the paper is completely affixed to the prison.baking with 150-160 degrees,5-8 minutes transfer (to avoid strong winds) and stay cool and spilled transfer paper, available after the blisters erase residual scraps of paper.
3. After cleaning, dry water, If there is residual glue watermark ,baking again with 120 degrees 5 minutes ,to remove traces of glue.
4. if necessary, then spray transparent light oil (cover light oil).
2. THE ADVANTAGES OF Hsinda :
|
|
|
|
|
|
|
3. the Advance of Hsinda Products
better resin from DSM | better pigment provide a good voverage and weather resist |
higher coverage | lower necessary thickness |
higher resin percentage | stable quality for each order |
the Advance of Hsinda Services
products customize |
7*24 hours online |
comprehensive cost analysis |
powder coating quality control system build |
Application
Electrical Household Appliances | Aerospace Area |
Automotive Electronics | Fitness Equipment |
Track Traffic | Medical Devices |
Petroleum Pipes, Valve | Tools & Hardware |
LED Lights, Outdoor Lamps | Radiator & Heat Sink |
Glass Decoration | External Facilities |
Powder Coating Spray
FAQ
1, what's the moq for the first time ?
for the first time , any quantity will be acceptable , but to save your ship cost . few kgs will be good. formal order moq will be 300kg per color .
2, could you do OEM for us ?
yes , we can do OEM for a distributor if you want , but may require a order more than 10 tons.